BASF Lupranate® LP30D Isocyanate

Category Fluid
Manufacturer BASF
Trade Name Lupranate®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Lupranate® LP30D Isocyanate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Lupranate® LP30D isocyanate is a solvent-free, modified pure diphenylmethane diisocyanate which is liquid at 30°C. It is designed to replace pure MDI in applications where it is desirable to use a product that can be stored as a liquid. It is used as a major starting material in applications such as prepolymers, elastomers, shoe soles, sealants and adhesives. The "D" stands for the drum packaging.Information provided by BASF
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Viscosity 16 cP
16 cP
Vapor Pressure 1.33e-8 bar

@Temperature 25.0 °C
0.00000998 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Boiling Point >= 190 °C

@Pressure 0.000667 MPa
>= 374 °F

@Pressure 0.0967 psi
Flash Point 200 °C
392 °F
Descriptive Properties Value Comments
Color Pale Yellow
Composition NCO content
0.33