Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF E-por® 0.025 g/cc Density; Styrene and Ethylene (Europe)

Category Polymer , Thermoplastic , Polyethylene (PE) , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer BASF
Trade Name E-por®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF E-por® 0.025 g/cc Density; Styrene and Ethylene (Europe).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing expanded foams.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.0160 - 0.0350 g/cc
0.000578 - 0.00126 lb/in³
Density 0.0250 g/cc
0.000903 lb/in³
Mechanical Properties Metric English Comments
Tensile Stress 0.100 MPa
14.5 psi
0.150 MPa
21.8 psi
0.200 MPa
29.0 psi
0.300 MPa
43.5 psi
0.625 MPa
90.6 psi
Flexural Strength 0.237 MPa
34.4 psi
0% E-por Content; DIN 53423
0.247 MPa
35.8 psi
60% E-por Content; DIN 53423
0.257 MPa
37.3 psi
100% E-por Content; DIN 53423
0.330 MPa
47.9 psi
DIN-EN 12089
Compressive Strength 0.115 MPa

@Strain 10.0 %
16.7 psi

@Strain 10.0 %
DIN-EN 826
0.145 MPa

@Strain 25.0 %
21.0 psi

@Strain 25.0 %
DIN-EN 826
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Descriptive Properties Value Comments
Commercial Status Europe
Cushioning 2.73
h/d=15; DIN 55471
Energy Absorption 12.5 J
Hysteresis at 70% compression, v=% mm/min; ISP 3386-1
Flexural Work to Break 0.227
0% E-por Content; DIN 53423
0.247
60% E-por Content; DIN 53423
0.25
100% E-por Content; DIN 53423
6.3 J
DIN-EN 12098