Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 47H BK0501 was formulated to provide thermal endurance when used in applications in which continuous or extended high-temperature exposure is anticipated. Vydyne 47H BK0501 is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact strength. This resin offers a well balanced combination of engineering properties characterized by high melt point, good surface lubricity, abrasion resistance and resistance to many chemicals, machine and motor oils, solvents and gasoline. Vydyne 47H BK0501 is designed to meet the critical low-temperature impact requirements called out in many automotive specifications. Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline ResistanceGeneral Purpose Good Abrasion ResistanceGood Chemical Resistance Good ProcessabilityGood ToughnessHigh Impact ResistanceImpact ModifiedLow Temperature Impact Resistance Low Temperature ToughnessOil ResistantSolvent ResistantUses: Automotive ApplicationsConnectorsConsumer ApplicationsElectrical/Electronic ApplicationsFastenersGearsIndustrial Applications Appearance: BlackForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.3 %
2.3 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Diameter 2.00 mm
0.018 in/in

@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Diameter 2.00 mm
0.016 in/in

@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527-2
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527-2
Elongation at Break >= 60 %
>= 60 %
ISO 527-2
Tensile Modulus 1.74 GPa
252 ksi
ISO 527-2
Flexural Strength 24.0 MPa
3480 psi
ISO 178
Flexural Modulus 0.780 GPa
113 ksi
ISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²

@Temperature -40.0 °C
8.57 ft-lb/in²

@Temperature -40.0 °F
ISO 180
24.0 kJ/m²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180
44.0 kJ/m²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.80 J/cm²

@Temperature -40.0 °C
8.57 ft-lb/in²

@Temperature -40.0 °F
ISO 179
2.40 J/cm²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179
6.20 J/cm²

@Temperature 23.0 °C
29.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179