| Category | Fluid , Solvent |
| Manufacturer | Asahi Glass Company |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Asahi Glass CFC-113 Chlorofluorocarbon Solvent.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.007398 g/cc @Temperature 50.0 °C |
0.0002673 lb/in³ @Temperature 122 °F |
Vapor (1 atm) |
| 1.57 g/cc @Temperature 25.0 °C |
0.0567 lb/in³ @Temperature 77.0 °F |
Liquid | |
| Solubility of Water | 0.019 % | 0.019 % | 25°C |
| Solubility in Water | 0.017 % | 0.017 % | 25°C |
| Viscosity | 0.65 cP @Temperature 25.0 °C |
0.65 cP @Temperature 77.0 °F |
|
| Molecular Weight | 187.38 g/mol | 187.38 g/mol | |
| Vapor Pressure | 0.448 bar @Temperature 25.0 °C |
336 torr @Temperature 77.0 °F |
|
| Surface Tension | 17.3 dynes/cm | 17.3 dynes/cm | 25°C |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Heat of Vaporization | 151 J/g | 65.0 BTU/lb | b.p. |
| Specific Heat Capacity | 0.708 J/g-°C @Temperature 50.0 °C |
0.169 BTU/lb-°F @Temperature 122 °F |
Vapor (1atm) |
| 0.962 J/g-°C @Temperature 25.0 °C |
0.230 BTU/lb-°F @Temperature 77.0 °F |
Liquid | |
| Melting Point | -35.0 °C | -31.0 °F | |
| Boiling Point | 47.6 °C | 118 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.356 @Temperature 23.0 °C |
1.356 @Temperature 73.4 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 2.41 @Frequency 1e+6 Hz |
2.41 @Frequency 1e+6 Hz |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Critical Pressure | 34.12 bar | 25590 torr | |
| Critical Temperature | 214.36 °C | 417.85 °F | |
| Critical Density | 0.570 g/cc | 0.0206 lb/in³ |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Global Warming Potential (CO2=1, 100yr ITH) | 5000 | |
| KB Value | 31 | |
| Ratio of Specific Heat Cp/Cv 60C 1atm | 1.096 | |
| Relative Evaporation Rate (ether=100) | 123 |