Arkema Group Rilsan® BESN P40 W5 TL Nylon 11, Flexible Tubing Grade (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Flexible Tubing Grade
Manufacturer Arkema
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® BESN P40 W5 TL Nylon 11, Flexible Tubing Grade (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Designation ISO 1874-PA11-P,EFHL,22-003Flexible grade for tubes extrusion. Available color: milky white. Light and heat stabilized. Flame retardant agent.Fire-resistant. Flexibility. High impact strength. Very good chemical resistance. Ability to be processed at high speed.Example applications: Flexible tubes for automotive.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
Water Absorption 1.4 %
1.4 %
Melt Flow 7.9 g/10 min

@Load 2.16 kg,
Temperature 235 °C
7.9 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 38 %
38 %
50 mm/min
Tensile Modulus 0.605 GPa
87.7 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 3.80 J/cm²
18.1 ft-lb/in²
Partial Break
0.430 J/cm²

@Temperature -30.0 °C
2.05 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Oxygen Index 27 %