Category | Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE |
Manufacturer | AlphaGary |
Trade Name | Evoprene™ GC |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | AlphaGary Evoprene™ GC 5694 SEBS Thermoplastic Elastomer.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ISO 2782 |
Viscosity Measurement | 6.0 @Temperature 180 °C |
6.0 @Temperature 356 °F |
Kg/cm<sup>2</sup>; Macklow-Smith extrusion rheometer |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 25 | 25 | ISO 868 |
Tensile Strength | 2.40 MPa | 348 psi | ISO 37 |
Elongation at Break | 750 % | 750 % | ISO 37 |
100% Modulus | 0.000500 GPa | 0.0725 ksi | ISO 37 |
Tear Strength | 13.0 kN/m | 74.2 pli | ISO 34-B |
Compression Set | 33 % @Temperature 70.0 °C, Time 79200 sec |
33 % @Temperature 158 °F, Time 22.0 hour |
ISO 815 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -60.0 - -50.0 °C | -76.0 - -58.0 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Bonds with | Polypropylene | |
Chemical Resistance | Acetone | Moderate |
Acids up to 80% | Good | |
Alcohol | Good | |
Alkalis | Good | |
Brake fluid | Moderate | |
Chlorinate solvents | Poor | |
Diesel | Poor | |
Ethylene glycol | Excellent | |
Gasoline | Poor | |
Salt solution | Good | |
Soda lye | Good | |
Water, 23°C | Excellent | |
Water, 95°C | Moderate | |
Transparency | Opaque |