Material Notes:
Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades bond to polycarbonate, ABS, polycarbonate/ABS alloys, SAN, ASA, copolyester elastomers and TPUs, as well as both flexible and rigid PVC. Applications:Injection-molded and overmolded partsSoft touch handles and gripsAutomotive interior applicationsSeals and gaskets for automotive insert moldingNoise and vibration deadeningBlow-molded partsTubing and hoseWire and cable jacketsCoated fabrics and sheet goodsWindow and door weatherstrippingInformation provided by Advanced Polymer Alloys
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D471
Viscosity 455000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
455000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
After 7 days at 125°C; ASTM D573
79
79
ASTM D2240
Tensile Strength at Break 12.30 MPa
1784 psi
ASTM D412
14.39 MPa
2087 psi
After 7 days at 125°C; ASTM D573
Elongation at Break 560 %
560 %
ASTM D412
599.2 %
599.2 %
After 7 days at 125°C; ASTM D573
100% Modulus 0.00448 GPa
0.650 ksi
ASTM D412
0.00547 GPa
0.793 ksi
After 7 days at 125°C; ASTM D573
Graves Tear Strength 61.02 kN/m

@Temperature 24.0 °C
348.1 pli

@Temperature 75.2 °F
Die C; ASTM D624
Compression Set 22 %
22 %
After 22 Hr At 24°C; ASTM D395
89 %
89 %
After 22 Hr at 100°C; ASTM D395
Tensile Set 17 %
17 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -58.0 °C
-72.4 °F
ASTM D746
Clash Berg Stiffness Temperature -22.0 °C
-7.60 °F
69 Mpa; ASTM D1043
Processing Properties Metric English Comments
Processing Temperature 177 °C
351 °F
Descriptive Properties Value Comments
Fluid Resistance - Volume Change, % (ASTM D471) 13
After 7 Days in IRM 903 Oil No. 3 at 212°F (100°C)
14
After 7 Days in Water at 212°F (100°C)
24
After 7 Days in ASTM Ref. Fuel no. B at 75°F (24°C)
-7
After 7 Days in ASTM Oil No. 1 At 212°F (100°C)
Users viewing this material also viewed the following: