Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AdvanSource Biomaterials ChronoPrene™ 25A Thermoplastic Rubber Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer AdvanSource Biomaterials (formerly CardioTech International)
Trade Name ChronoPrene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AdvanSource Biomaterials ChronoPrene™ 25A Thermoplastic Rubber Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ChronoPrene™ is a family of biocompatible thermoplastic elastomeric materials.ChronoPrene™ is a family of easy molding, high flow rubber, with excellent chemical resistance to alcohols, acids, and bases. ChronoPrene™ is offered as a translucent resin in a durometer hardness of 5 - 40 Shore A. The outstanding characteristic of this family of compounds is their ability to be injection molded at temperatures between 175ºC and 235ºC. The result is an injected molded part with very good surface smoothness and excellent elasticity.ChronoPrene™ elastomeric resins are thermoplastic rubbers, which can be extruded or molded by standard thermoplastic processing equipment. Most traditional rubbers are thermosetting in nature, often making them difficult to compound, mold, and are not always biocompatible.Information provided by AdvanSource Biomaterials Corporation.
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
3 sec.; ASTM D2240
Tensile Strength, Ultimate 4.14 MPa
600 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
Processing Properties Metric English Comments
Processing Temperature <= 127 °C
<= 260 °F
Upper stability limit
Mold Temperature -1.11 - 12.8 °C
30.0 - 55.0 °F
Warp-free parts
79.4 - 113 °C
175 - 235 °F
Maximum surface smoothness and rubberiness
Descriptive Properties Value Comments
Color Translucent