| Category | Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Mica Filled |
| Manufacturer | Adamas |
| Trade Name | Adalon® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Adamas Adalon® 453 PTFE, Mica filler.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.28 - 2.30 g/cc | 2.28 - 2.30 g/cc | ASTM D792 |
| Water Absorption | 0.030 % | 0.030 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 62 - 68 | 62 - 68 | ASTM D2240 |
| Ball Indentation Hardness | 100 - 115 MPa | 14500 - 16700 psi | ISO 2032 |
| Tensile Strength at Break | 9.00 - 11.0 MPa | 1310 - 1600 psi | ISO 527-1 |
| Elongation at Break | 40 - 60 % | 40 - 60 % | ISO 527-1 |
| Coefficient of Friction, Dynamic | 0.030 - 0.15 | 0.030 - 0.15 | ASTM D1894 |
| Coefficient of Friction, Static | 0.080 - 0.18 | 0.080 - 0.18 | ASTM D1894 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 327 °C | 621 °F | DSC |
| Maximum Service Temperature, Air | 260 °C | 500 °F | DSC |
| Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
| Dielectric Constant | 2.58 <br>@Frequency 60.0 - 2.00e+6 Hz |
2.58 <br>@Frequency 60.0 - 2.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 7.00 - 8.00 kV/mm | 178 - 203 kV/in | ASTM D149 |