| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Accutech Polypropylene Copolymer CP0437T40L1 Talc Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | MD; ASTM D955 |
| Melt Flow | 14 g/10 min | 14 g/10 min | ASTM D1238 |
| Ash | 40 % | 40 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 42 | 42 | ASTM D785 |
| Tensile Strength at Break | 16.0 MPa | 2320 psi | ASTM D638 |
| Tensile Strength, Yield | 18.0 MPa | 2610 psi | ASTM D638 |
| Elongation at Break | 6.0 % | 6.0 % | ASTM D638 |
| Elongation at Yield | 2.0 % | 2.0 % | ASTM D638 |
| Tensile Modulus | 2.099 GPa | 304.5 ksi | ASTM D638 |
| Flexural Strength | 20.0 MPa | 2900 psi | ASTM D790 |
| Flexural Modulus | 2.499 GPa | 362.5 ksi | ASTM D790 |
| Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 234 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 62.8 °C | 145 °F |