Material Notes:
Aluminum Nitride key properties: High thermal conductivity, Good resistance to abrasion and oxidation, Electrical insulating material, Low thermal expansion coefficient, PiezoelectricAluminum Nitride main applications domains: High temperature piezoelectric pressure sensors, Substrates for electronic packages, Opto-electronics: Deep UV LEDs, Heat sinks for the microelectronics, IC packages, Power transistor, Microwave device packages, Material processing kiln furniture, Semiconductor processing chamber fixtures and insulators, Molten metal handling components, Medical (echography)Information provided by Acerde
Physical Properties Metric English Comments
Density 3.26 g/cc
0.118 lb/in³
Mechanical Properties Metric English Comments
Vickers Microhardness 1100
1100
[Kg/mm²]
Flexural Strength 320 MPa
46400 psi
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature <=1000 °C
2.50 µin/in-°F

@Temperature <=1830 °F
Thermal Conductivity 285 W/m-K
1980 BTU-in/hr-ft²-°F
Melting Point 3200 °C
5790 °F
Under High Pressure