ATI Allvac® Nickelvac® D6AC UNS K24728 Specialty Steel

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer ATI Allvac
Trade Name Nickelvac®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Nickelvac® D6AC UNS K24728 Specialty Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Uses: High performance aircraft structural parts.Property values are for samples in the metallurgical condition: 1550°F Q + 1000°F T.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 7.78 g/cc
0.281 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 45
45
Tensile Strength, Ultimate 1483 MPa
215100 psi
Tensile Strength, Yield 1379 MPa

@Strain 0.200 %
200000 psi

@Strain 0.200 %
Elongation at Break 12 %
12 %
Reduction of Area 40 %
40 %
Component Elements Properties Metric English Comments
Carbon, C 0.48 %
0.48 %
Chromium, Cr 1.1 %
1.1 %
Iron, Fe 96 %
96 %
as balance
Manganese, Mn 0.80 %
0.80 %
Molybdenum, Mo 1.0 %
1.0 %
Nickel, Ni 0.60 %
0.60 %
Phosphorous, P 0.0050 %
0.0050 %
Silicon, Si 0.23 %
0.23 %
Sulfur, S 0.0050 %
0.0050 %
Vanadium, V 0.12 %
0.12 %