| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) |
| Manufacturer | ATG s.r.l. |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | ATG s.r.l. IIR Butyl Rubber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.920 g/cc | 0.920 g/cc |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 40 - 85 | 40 - 85 | |
| Tensile Strength, Ultimate | 7.00 - 18.0 MPa | 1020 - 2610 psi | |
| Elongation at Break | 250 - 800 % | 250 - 800 % | |
| Rebound | 6.0 - 12 % | 6.0 - 12 % |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 120 °C | 248 °F | |
| Minimum Service Temperature, Air | -30.0 °C | -22.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Abrasion Resistance | medium | |
| Chemical Resistance to Animal and Vegetable Oils and Greases | medium | |
| Chemical Resistance to Aromatic Hydrocarbons | none | |
| Chemical Resistance to Chloride Solvents | none | |
| Chemical Resistance to Distilled Water | high | |
| Chemical Resistance to Ketones | high | |
| Chemical Resistance to Maximum Concentrated Alkalis (at 50°C) | high | |
| Chemical Resistance to Medium-High Concentrated Acids (at 50°C) | medium | |
| Chemical Resistance to Mineral Oils and Aliphatic Hydrocarbons | none | |
| Compression set at 100°C | medium | |
| Impermeability at gas (Oxygen and Nitrogen) | medium | |
| Resistance to Flame | none | |
| Resistance to Heat Aging | low | |
| Resistance to Low Temperatures | low | |
| Resistance to Ozone and Weathering | medium | |
| Tear Strength | medium |