AK Steel 316 contains molybdenum. This addition increases general corrosion resistance, improves resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.99 g/cc
0.289 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 79
79
Tensile Strength, Ultimate 579 MPa
84000 psi
Tensile Strength, Yield 290 MPa

@Strain 0.200 %
42100 psi

@Strain 0.200 %
Elongation at Break 50 %
50 %
in 2 inches
Modulus of Elasticity 193 GPa
28000 ksi
tension
Poissons Ratio 0.25
0.25
Calculated
Shear Modulus 77.0 GPa
11200 ksi
torsion
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C

@Temperature 0.000 - 100 °C
8.89 µin/in-°F

@Temperature 32.0 - 212 °F
19.9 µm/m-°C

@Temperature <=871 °C
11.1 µin/in-°F

@Temperature <=1600 °F
Specific Heat Capacity 0.500 J/g-°C

@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F

@Temperature 32.0 - 212 °F
Thermal Conductivity 16.2 W/m-K

@Temperature 100 °C
112 BTU-in/hr-ft²-°F

@Temperature 212 °F
21.4 W/m-K

@Temperature 500 °C
149 BTU-in/hr-ft²-°F

@Temperature 932 °F
Melting Point 1371 - 1399 °C
2500 - 2550 °F
Solidus 1371 °C
2500 °F
Liquidus 1399 °C
2550 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Chromium, Cr 16 - 18 %
16 - 18 %
Iron, Fe 61.995 - 72 %
61.995 - 72 %
As Remainder
Manganese, Mn <= 2.0 %
<= 2.0 %
Molybdenum, Mo 2.0 - 3.0 %
2.0 - 3.0 %
Nickel, Ni 10 - 14 %
10 - 14 %
Nitrogen, N <= 0.010 %
<= 0.010 %
Phosphorous, P <= 0.045 %
<= 0.045 %
Silicon, Si <= 0.75 %
<= 0.75 %
Sulfur, S <= 0.030 %
<= 0.030 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000740 ohm-cm
0.0000740 ohm-cm
Magnetic Permeability <= 1.02
<= 1.02
H = 200 Oersteds, Annealed