Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Hiloy® 130 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled, UL

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 130 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled, UL.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Ultimate 95.0 MPa
13800 psi
ASTM D638
Elongation at Break 2.6 %
2.6 %
ASTM D638
Flexural Strength 137 MPa
19900 psi
ASTM D790
Flexural Modulus 7.00 GPa
1020 ksi
ASTM D790
Izod Impact, Notched 0.910 J/cm
1.70 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.87 J/cm
11.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 163 °C
325 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 152 °C
306 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 225 °C
437 °F
Approximate middle barrel temperature.