Material Notes:
Scotchkote Epoxy Metal Repair EG 503 is a specifically developed high performance metal compound that provides good mechanical strength combined with easy machining properties.Product Features:Combines good machining characteristics with good mechanical propertiesDesigned for application by trowel or spatula at thicknesses up to 12 mmProvides outstanding cold weld capabilitiesDesigned for use to repairs to cracked casting and rebuilding worn shafts, bearing housings and flangesExcellent adhesion to correctly prepared metal surface.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Thickness 11900 microns
470 mil
Mechanical Properties Metric English Comments
Flexural Strength 68.9 MPa
10000 psi
Compressive Strength 107 MPa
15500 psi
Shear Strength 17.2 MPa
2500 psi
Tensile Shear Adhesion
Thermal Properties Metric English Comments
Heat Distortion Temperature 90.0 °C
194 °F
post cured 24 hrs at 100°C
Processing Properties Metric English Comments
Cure Time 60.0 min
1.00 hour
Initial Set
4320 min
72.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Gray