3M Scotch-Weld™ MG20 SF Medical Grade Instant Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ MG20 SF Medical Grade Instant Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plastics, rubbers, and composite materials and are available with special properties such as fast cure, low odor, flexibility and a variety of viscosities. This product has been tested and meets the specifications of USP Class VI. These products are not intended for use in implantable medical assemblies or for direct application to the skin. MG20 SF is a fast curing cyanoacrylates that rely less on surface moisture for cure speed than standard cyanoacrylates. These cyanoacylates can be used for a super fast cure in high speed production applications. Scotch-Weld Medical Grade Instant Adhesives MG20 SF is a low viscosity instant adhesive that will bond close-fitting partsInformation provided by 3M
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Viscosity 17 - 22 cP
17 - 22 cP
ISO 3104/3105
Mechanical Properties Metric English Comments
Tensile Strength at Break 33.1 MPa
4800 psi
cured, grit-blasted steel; ASTM D2095
Shear Strength 20.7 MPa
3000 psi
Overlap, grit-blasted steel; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.0500 - 0.500 min
0.000833 - 0.00833 hour
Time to Handling
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Liquid