3M Scotch® 8621 Tear Strip Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 8621 Tear Strip Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Scotch® Tear Strip 8621 is a high-performance tape reinforced with continuous polypropylene monofilaments. It is designed as an easy-opening tear strip tape for light-duty paperboard, which can be applied with a flat surface or vacuum wheel applicator.Information provided by 3M
Mechanical Properties Metric English Comments
Elongation at Break 30 %
30 %
ASTM D3759
Peel Strength 0.701 kN/m
4.00 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Pressure-sensitive synthetic rubber resin
Appearance White