Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotch® 3734 Printed Message Box Sealing Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 3734 Printed Message Box Sealing Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Scotch® Box Sealing Tape 3734 is a polypropylene carton sealing tapes. A high performance box sealing tape with a strong backing and an aggressive adhesive that provides a secure and durable closure. A box sealing tape that can be custom printed to provide security and/or branding. A carton sealing tape that provides high quality, consistent performance with easy unwind.Information provided by 3M
Physical Properties Metric English Comments
Thickness 63.5 microns
2.50 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 8.75 MPa
1270 psi
Elongation at Break 160 %
160 %
Peel Strength 0.5478 kN/m
3.125 pli
Adhesion to Steel
Descriptive Properties Value Comments
Adhesive Type Hot Melt Synthetic Rubber Resin
Appearance Tan
Users viewing this material also viewed the following: