Material Notes:
3M™ Dyneon™ Flouroelastomer FC 2121 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, Dyneon FC 2121 should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks have good scorch resistance and storage stability.Composition: di-polymer of vinylidene fluoride and hexafluoropropyleneLow viscosityProcess targets: injection and transfer molding, extrusion and calenderingProprietary incorporated cure technologyUtilizes FC 2174 cure technologyInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Mooney Viscosity 24

@Temperature 121 °C
24

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.38 MPa
2375 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 180 %
180 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 0.007067 GPa
1.025 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 14 %
14 %
Aged 70 hours @ 200°C, O-rings -214; ASTM D395 Method B
Thermal Properties Metric English Comments
Transformation Temperature -18.0 °C
-0.400 °F
TR10; ASTM D1329
Component Elements Properties Metric English Comments
Fluorine, F 65.9 %
65.9 %
Descriptive Properties Value Comments
Color Opaque Off-White
MH, Maximum Torque 21 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
22 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
ML, Minimum Torque 0.7 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
0.8 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
Solubility Ketones and Esters
t`50, Time to 50% cure 0.6 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
1.6 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
t`90 - Time to 90% cure 0.8 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
2.3 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
ts2 - Time to 2 in-lb rise from min 0.5 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
1.4 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289