Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M CC-2 Cable Cleaning Preparation Kits

Category Fluid , Solvent
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M CC-2 Cable Cleaning Preparation Kits.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Formulated to exhibit excellent cleaning and degreasing properties. CC series solvent is a colorless non-conducting liquid that emanates a light orange peel scent. It is compatible with all solid dielectric cable insulations, will not cause tracking on insulation surfaces. Accelerated surface drying can be accomplished by applying forced air or by wiping dry with a clean cloth. Use of solvent on carbon containing semi-conductive surfaces such as cable insulation shields is no recommended. There are three solvent containing products with in the CC series to meet cleaning needs as follows: CC-2 Cable Cleaning Preparation Kits, CC-3 Cable Cleaning Pad Kits and CC-4 Cable Cleaning Solvent.Information provided by 3M
Physical Properties Metric English Comments
Density 0.760 g/cc
0.0275 lb/in³
Volatiles 100 %
100 %
Vapor Pressure 0.000267 bar
0.200 torr
Thermal Properties Metric English Comments
Boiling Point 193 - 249 °C
379 - 480 °F
Flash Point 62.0 °C
144 °F
Closed Cup
74.0 °C
165 °F
Open Cup
Electrical Properties Metric English Comments
Dielectric Strength 19.7 kV/mm
500 kV/in
1/2" dia spheres; ASTM D877-87
Descriptive Properties Value Comments
Appearance Colorless Liquid