3M 1126 EMI Shielding Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF 3M 1126 EMI Shielding Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by 3M
Physical Properties Metric English Comments
Thickness 35.6 microns
1.40 mil
Backing
88.9 microns
3.50 mil
Total
Mechanical Properties Metric English Comments
Peel Strength 0.394 kN/m
2.25 pli
Adhesion to steel; ASTM D1000