PRODUCT NO. Category Trade Name
SIDPEC EGYPTENE® HD 3802 FA HDPE Film High Density Polyethylene (HDPE), Film Grade EGYPTENE®
SIDPEC EGYPTENE® HD 4602 FA HDPE Film High Density Polyethylene (HDPE), Film Grade EGYPTENE®
SIDPEC EGYPTENE® HD 5211 EA HDPE Injection Molding High Density Polyethylene (HDPE), Injection Molded EGYPTENE®
SIDPEC EGYPTENE® HD 5218 EA HDPE Injection Molding High Density Polyethylene (HDPE), Injection Molded EGYPTENE®
SIDPEC EGYPTENE® HD 5226 EA HDPE Injection Molding High Density Polyethylene (HDPE), Injection Molded EGYPTENE®
SIDPEC EGYPTENE® HD 5301 EA HDPE Blow Molding High Density Polyethylene (HDPE), Blow Molding Grade EGYPTENE®
SIDPEC EGYPTENE® HD 5301 FB HDPE Film High Density Polyethylene (HDPE), Film Grade EGYPTENE®
SIDPEC EGYPTENE® HD 5402 EA HDPE Pipe Grade High Density Polyethylene (HDPE), Pipe Grade EGYPTENE®
SIDPEC EGYPTENE® HD 5403 EA HDPE Blow Molding High Density Polyethylene (HDPE), Blow Molding Grade EGYPTENE®
SIDPEC EGYPTENE® HD 5420 GA HDPE Blow Molding High Density Polyethylene (HDPE), Blow Molding Grade EGYPTENE®
SIDPEC EGYPTENE® HD 5813 EA HDPE Injection Molding High Density Polyethylene (HDPE), Injection Molded EGYPTENE®
SIDPEC EGYPTENE® HD 6070 UA HDPE Injection Molding High Density Polyethylene (HDPE), Injection Molded EGYPTENE®
SIDPEC EGYPTENE® HD 5502 GA HDPE Blow Molding High Density Polyethylene (HDPE), Blow Molding Grade EGYPTENE®
SIDPEC EGYPTENE® HD 5740 UA HDPE Injection Molding High Density Polyethylene (HDPE), Injection Molded EGYPTENE®