HOME
ABOUT US
PRODUCT
Thermoplastic
Thermoset
Adhesive
RenewableRecycled-Polymer
RenewableRecycled-Film
Tape
RECENT UPDATE
Company News
Product News
CONTACT US
RFQ
POLYMER SEARCH
SEARCH
HOME
POLYMER SEARCH
Polyram
Polyram > Polypropylene with 20% Glass Fiber Filler
Manufacturer :
Polyram
>
Category :
Polypropylene with 20% Glass Fiber Filler
Product List
Tips:
100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO.
Category
Trade Name
Polyram Polytron P20B11 Polypropylene, 20% Long Fiber Glass
Polypropylene with 20% Glass Fiber Filler
Polytron
Polyram RamOfin PPH302G4 Polypropylene, 20% Glass Fiber
Polypropylene with 20% Glass Fiber Filler
Polyram RamOfin PPH316G4 Polypropylene, 20% Glass Fiber
Polypropylene with 20% Glass Fiber Filler
Polyram RamOfin PPH501G4 Polypropylene, 20% Glass Fiber, Flame Retardant
Polypropylene with 20% Glass Fiber Filler
Polyram Polytron P20B01 Homopolymer Polypropylene, Chemically Coupled 20% Long Fiber
Polypropylene with 20% Glass Fiber Filler
Polytron
Polyram Polytron P20B03 Polypropylene, 20% Long Glass Fiber
Polypropylene with 20% Glass Fiber Filler
Polytron
Polyram RamOfin PPH300G3 Polypropylene, 15% Glass Fiber
Polypropylene with 20% Glass Fiber Filler
Polyram RamOfin PPH300G4 Polypropylene, 20% Glass Fiber
Polypropylene with 20% Glass Fiber Filler