PRODUCT NO. Category Trade Name
Polykemi AB SCANTEC PC S60R GF10 V0 Polycarbonate, Glass-Fiber Reinforced, Flame Retardant Polycarbonate, 10% Glass Filled SCANTEC
Polykemi AB SCANTEC PC S60R GF20 V0 Polycarbonate, Glass-Fiber Reinforced, Flame Retardant Polycarbonate, 20% Glass Filled SCANTEC
Polykemi AB SCANTEC PC S60R GF30 V0 Polycarbonate, Glass-Fiber Reinforced, Flame Retardant Polycarbonate, 30% Glass Filled SCANTEC
Polykemi AB SCANTEC PC S75R GF20 V0 Polycarbonate, Glass Fiber Reinforced, Flame Retardant Polycarbonate, 20% Glass Filled SCANTEC
Polykemi AB SCANTEC PC S75R GF10 V0 Polycarbonate, Glass Fiber Reinforced, Flame Retardant Polycarbonate, 10% Glass Filled SCANTEC
Polykemi AB SCANTEC PC S75R GF30 V0 Polycarbonate, Glass Fiber Reinforced, Flame Retardant Polycarbonate, 30% Glass Filled SCANTEC