PRODUCT NO. Category Trade Name
LATI Lastilac AR G/17-V0E ABS, 17% Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled Lastilac
LATI Lastilac SP G/17 ABS, Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled Lastilac
LATI Latiohm 36/07 PD01 G/20 ABS, 20% Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled Latiohm