PRODUCT NO. Category Trade Name
Cadi 100W Tungsten Pure Element
Cadi 10TC Tungsten Carbide Copper Tungsten Alloy
Cadi 10WA Tungsten Copper Alloy Tungsten Alloy
Cadi 10WC Tungsten Copper Tungsten Alloy
Cadi 15WC Tungsten Copper Tungsten Alloy
Cadi 1WC Tungsten Copper Tungsten Alloy
Cadi 20TC Tungsten Carbide Copper Tungsten Alloy
Cadi 20WS Tungsten Silver Silver Alloy
Cadi 30WC Tungsten Copper Tungsten Alloy
Cadi 35WS Tungsten Silver Silver Alloy
Cadi 3WC Tungsten Copper Tungsten Alloy
Cadi 50WS Tungsten Silver Silver Alloy
Cadi 5TC Tungsten Carbide Copper Copper Alloy
Cadi 5WC Tungsten Copper Tungsten Alloy
Cadi Cu-Tungsten (55%) Copper Alloy Tungsten Alloy
Cadi Cu-Tungsten (75%) Copper Alloy Tungsten Alloy
Cadi Cu-Tungsten (80%) Copper Alloy Tungsten Alloy
Cadi TCWA Tungsten Carbide Copper Alloy Tungsten Alloy
Cadi Tungsten Pure Element