Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : Buckeye Polymers > Category : Polypropylene with 20% Talc Filler Product List

Tips:100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Category Trade Name
Buckeye Polymers BP RPP 2020T Polypropylene, 20% Mineral Filled Polypropylene with 20% Talc Filler
Buckeye Polymers BP RPP 2006 T Polypropylene, 20% Mineral Filled Polypropylene with 20% Talc Filler
Buckeye Polymers BP RPP 2008 T NAT Polypropylene, Talc Filled Polypropylene with 20% Talc Filler
Buckeye Polymers BP RPP 2010 T NAT Polypropylene, Talc Filled Polypropylene with 20% Talc Filler
Buckeye Polymers BP RPP 2012 TR BLK Polypropylene, Talc Filled Polypropylene with 20% Talc Filler
Buckeye Polymers BP RPPC 1720 TURXF Polypropylene, Talc Filled Polypropylene with 20% Talc Filler
Buckeye Polymers BP RPP 2007 TR Blk Reprocessed Polypropylene, 20% Mineral Filled Renewable/Recycled Polymer
Buckeye Polymers BP RPP 2012 T BLK Polypropylene, Talc Filled Polypropylene with 20% Talc Filler
Copyright © lookpolymers.com All Rights Reserved