Addiplast Addinyl B2 ZG30 Nylon 6, 30% Glass Bead Nylon 6, Glass Bead Filled Addinyl
Addiplast Addinyl B2H G30 Flame Retardant Nylon 6, 30% Glass Bead Nylon 6, Glass Bead Filled Addinyl
Addiplast Addinyl B2 G30 Nylon 6, 30% Glass Bead Nylon 6, Glass Bead Filled Addinyl
Addiplast Addinyl B2H G15 Flame Retardant Nylon 6, 15% Glass Bead Nylon 6, Glass Bead Filled Addinyl