Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+7 ohm-cm @Temperature 250 °C |
1.00e+7 ohm-cm @Temperature 482 °F |
DIN 52326 |
Schott Nextrema® 712-3 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm @Temperature 250 °C |
1.00e+7 ohm-cm @Temperature 482 °F |
DIN 52326 |
Schott Nextrema® 724-5 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm @Temperature 250 °C |
1.00e+7 ohm-cm @Temperature 482 °F |
DIN 52326 |
Schott Nextrema® 724-8 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm @Temperature 500 °C |
1.00e+7 ohm-cm @Temperature 932 °F |
|
CeramTec Frequenta® Steatite Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. Frequenta® has low dielectric loss, but has be.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm @Temperature 600 °C |
1.00e+7 ohm-cm @Temperature 1110 °F |
ASTM-D1829 |
CeramTec Rubalit® 600 Alumina, 48% Rubalit® 600 is suitable for both mechanical and laser trimming and is chiefly used as the core for high-grade carbon-film resistors. |
|||
Volume Resistivity | >= 1.00e+7 ohm-cm @Temperature 800 °C |
>= 1.00e+7 ohm-cm @Temperature 1470 °F |
|
CeramTec Rubalit® A 1894 Alumina, 94% Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |
|||
Volume Resistivity | >= 1.00e+7 ohm-cm @Temperature 800 °C |
>= 1.00e+7 ohm-cm @Temperature 1470 °F |
IEC 672-1 |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm @Temperature 400 °C |
1.00e+7 ohm-cm @Temperature 752 °F |
IEC 345 |
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate) Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua.. |
|||
Volume Resistivity | >= 1.00e+7 ohm-cm @Temperature 800 °C |
>= 1.00e+7 ohm-cm @Temperature 1470 °F |
IEC 672-1 |
CeramTec Rubalit® IS 95 Alumina Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva.. |
|||
Volume Resistivity | >= 1.00e+7 ohm-cm @Temperature 700 °C |
>= 1.00e+7 ohm-cm @Temperature 1290 °F |
ASTM-D1829 |
CoorsTek ADS-995R MidFilm™ 99.5% Alumina Thick Film Applications: thick films and lasers |
|||
Volume Resistivity | 1.00e+7 ohm-cm @Temperature 175 °C |
1.00e+7 ohm-cm @Temperature 347 °F |
ASTM D257 |
3M Scotchcast™ 265 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 265 is a new solution to an old problem. Historically, manufactures of coils, stators and armatures have used liquid-based varnishes or resins to coat and impregnate t.. |
|||
Volume Resistivity | >= 1.00e+7 ohm-cm @Temperature 800 °C |
>= 1.00e+7 ohm-cm @Temperature 1470 °F |
IEC 672-1 |
CeramTec Rubalit® A 1896 Alumina Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele.. |
|||
Volume Resistivity | >= 1.00e+7 ohm-cm @Temperature 800 °C |
>= 1.00e+7 ohm-cm @Temperature 1470 °F |
|
CeramTec Rubalit® A 1898 Alumina, 98% Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |