Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+10 ohm-cm @Temperature 250 °C |
2.00e+10 ohm-cm @Temperature 482 °F |
|
Schott Glass 8270 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elem.. |
|||
Volume Resistivity | >= 2.00e+10 ohm-cm @Temperature 70.0 °C |
>= 2.00e+10 ohm-cm @Temperature 158 °F |
|
Sibur 140-13 Compound 230/1 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Volume Resistivity | 2.00e+10 ohm-cm @Temperature 500 °C |
2.00e+10 ohm-cm @Temperature 932 °F |
ASTM-D1829 |
CoorsTek AD-996 99.6% Alumina |
|||
Volume Resistivity | 2.00e+10 ohm-cm @Temperature 250 °C |
2.00e+10 ohm-cm @Temperature 482 °F |
|
Corning 7056 Alkali Borosilicate Crushed/Powdered Glass Crushed/Powdered glass available in mesh sizes 4 through 325 and can be customized. Used primarily as a Kovar Sealing Glass. This product is used in MOEMS applications. Information provided by Corn.. |