Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7.10e+13 ohm-cm | 7.10e+13 ohm-cm | 50%RH; IEC 60093 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK261 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology only from DuPont it provides exceptional welding resistanceInformation .. |
|||
Volume Resistivity | 7.10e+13 ohm-cm | 7.10e+13 ohm-cm | |
Dow Corning 3-4207 DIELECTRIC TOUGH GEL KIT Two-part, translucent green, fast RT or heat cure, tough, primerless chemical adhesion, UV indicator, and UL 94 V-1 flammability classification.Information provided by Dow Corning |