Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.10e+13 ohm-cm | 6.10e+13 ohm-cm | 60°C for 500 hrs |
Fujipoly Industries Sarcon® 30T Thin-Film TR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Volume Resistivity | 6.10e+13 ohm-cm | 6.10e+13 ohm-cm | 60°C for 500 hrs with 95% RH |
Fujipoly Industries Sarcon® 45U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |