Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.030 ohm-cm | 0.030 ohm-cm | |
Premix Thermoplastics PRESEAL 5020 Ni-Coated Graphite Highly conductive PRESEAL® thermoplastic elastomer compounds are injection-mouldable and extrudable plastics for EMI-gasket and -housing applications, among other uses. The material is an ideal cho.. |
|||
Volume Resistivity | 0.030 ohm-cm | 0.030 ohm-cm | |
Premix Thermoplastics PRESEAL 5020 Ni-Coated Graphite Metal replacement is one of the fastest growing areas for conductive plastics. Plastics, with their lighter weight, good processability and optimal combination of mechanical properties have challeng.. |
|||
Volume Resistivity | <= 0.030 ohm-cm | <= 0.030 ohm-cm | ISO Mil-G-835388 |
Premix Thermoplastics PRESEAL® TPE 5010 PRESEAL TPE 5010 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors or in grounding applica.. |
|||
Volume Resistivity | 0.030 ohm-cm | 0.030 ohm-cm | Mil-G-835388 |
Premix Thermoplastics PRESEAL® TPE 5020 General Description:PRESEAL® TPE 5020 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors o.. |
|||
Volume Resistivity | 0.030 ohm-cm | 0.030 ohm-cm | ASTM D257 |
Premix Thermoplastics PRESEAL® TPE 5020 General Description:PRESEAL® TPE 5020 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors o.. |
|||
Volume Resistivity | 0.030 ohm-cm | 0.030 ohm-cm | Aged; Chomerics MAT-1002 |
Parker Chomerics CHO-FORM 5537 EMI Shielding Material Fast Curing Form-in-Place EMI Shielding Material. Cho-Form 5537 is a one component, moisture cured, electrically conductive, form-in-place EMI gasketing material. The formulation contains nickel-pla.. |
|||
Volume Resistivity | <= 0.030 ohm-cm | <= 0.030 ohm-cm | |
Parker Chomerics Tecknit Consil®-E 811 Extruded Silver-Filled Silicone Elastomer Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se.. |
|||
Volume Resistivity | <= 0.030 ohm-cm | <= 0.030 ohm-cm | |
Parker Chomerics Tecknit Consil®-E 815 Extruded Silver-Filled Silicone Elastomer Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se.. |
|||
Volume Resistivity | 0.030 ohm-cm | 0.030 ohm-cm | Chomerics MAT-1002 |
Parker Chomerics CHO-FORM 5541 Conductive Form-In-Place Gaskets Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |