Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7.60e+13 ohm-cm | 7.60e+13 ohm-cm | |
Resinlab® EP1200 Black Casting Resin Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re.. |
|||
Volume Resistivity | 7.60e+13 ohm-cm | 7.60e+13 ohm-cm | |
Resinlab® EP1200LV Casting Resin Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility an.. |