Polymer Property : Volume Resistivity = 6.10e+13 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 6.10e+13 ohm-cm
6.10e+13 ohm-cm
60°C for 500 hrs
Fujipoly Industries Sarcon® 30T Thin-Film TR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Volume Resistivity 6.10e+13 ohm-cm
6.10e+13 ohm-cm
60°C for 500 hrs with 95% RH
Fujipoly Industries Sarcon® 45U Thin-Film UR
Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..