Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5000 ohm-cm | 5000 ohm-cm | Approximate value obtained from graphical representation; CTM E043 |
Nanocyl PLASTICYL™ PA1503 Polyamide 6 with 3 wt% of Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Volume Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
LATI Latamid 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Volume Resistivity | 5000 - 5.00e+6 ohm-cm | 5000 - 5.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON EX03319C PEI (Asia Pacific) LNP* Stat-Kon* EX03319C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Volume Resistivity | 5000 - 5.00e+6 ohm-cm | 5000 - 5.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON EX11318C PEI (Asia Pacific) LNP* Stat-Kon* EX11318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Volume Resistivity | 5000 - 5.00e+6 ohm-cm | 5000 - 5.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON EX08318C PEI (Asia Pacific) LNP* Stat-Kon* EX08318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Volume Resistivity | 5000 ohm-cm | 5000 ohm-cm | ASTM D991-89 |
Zotefoams Plastazote® LD32CN Conductive Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Volume Resistivity | 5000 ohm-cm | 5000 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® GC-4H PA*-CF40 Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo.. |
|||
Volume Resistivity | 5000 ohm-cm | 5000 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® GC-4H PA*-CF40 Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo.. |
|||
Volume Resistivity | 5000 ohm-cm | 5000 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat.. |
|||
Volume Resistivity | 5000 ohm-cm | 5000 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat.. |
|||
Volume Resistivity | 5000 ohm-cm | 5000 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30 Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab.. |
|||
Volume Resistivity | 5000 ohm-cm | 5000 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30 Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab.. |
|||
Volume Resistivity | 5000 ohm-cm | 5000 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® HT2C-3X black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X black 9833 us a 30% carbon-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc to ISO: PA 6T/66... |
|||
Volume Resistivity | 5000 ohm-cm | 5000 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® HT2C-3X black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X black 9833 us a 30% carbon-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc to ISO: PA 6T/66... |