Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.80e+14 ohm-cm | 3.80e+14 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Volume Resistivity | 3.80e+14 ohm-cm | 3.80e+14 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Volume Resistivity | 3.80e+14 ohm-cm | 3.80e+14 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Volume Resistivity | 3.80e+14 ohm-cm | 3.80e+14 ohm-cm | ASTM D257 |
Saint-Gobain Furon®, Kapton® K275 Tape Description: A 1 mil thermally conductive Kapton® film, coated on both sides with 2 mils of thermally-conductive pressure-sensitive adhesive. Recommended uses: Excellent for use in small, compact e.. |