Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 2.60e+16 ohm-cm | >= 2.60e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 4501 PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
Volume Resistivity | >= 2.60e+16 ohm-cm | >= 2.60e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 4501 PPC High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
Volume Resistivity | 2.60e+16 ohm-cm | 2.60e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ajedium™ KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 PEEK film is thermoplastic film that is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, high pu.. |
|||
Volume Resistivity | 2.60e+16 - 4.30e+16 ohm-cm | 2.60e+16 - 4.30e+16 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific .. |
|||
Volume Resistivity | 2.60e+16 - 4.30e+16 ohm-cm | 2.60e+16 - 4.30e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l.. |
|||
Volume Resistivity | 2.60e+16 ohm-cm @Thickness 3.00 mm |
2.60e+16 ohm-cm @Thickness 0.118 in |
IEC 60093 |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Volume Resistivity | 2.60e+16 - 3.60e+16 ohm-cm | 2.60e+16 - 3.60e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Volume Resistivity | 2.60e+16 - 3.60e+16 ohm-cm | 2.60e+16 - 3.60e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Volume Resistivity | 2.60e+16 - 3.60e+16 ohm-cm | 2.60e+16 - 3.60e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Volume Resistivity | 2.60e+16 - 3.60e+16 ohm-cm | 2.60e+16 - 3.60e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Volume Resistivity | 2.60e+16 - 3.60e+16 ohm-cm | 2.60e+16 - 3.60e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Volume Resistivity | 2.60e+16 - 3.60e+16 ohm-cm | 2.60e+16 - 3.60e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |