Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 0.070 ohm-cm | <= 0.070 ohm-cm | |
Epoxy Technology EPO-TEK® N20E Electrically Conductive Paste Product Description: EPO-TEK® N20E is a two component, electrically and thermally conductive, epoxy adhesive designed for semiconductor and electronics assembly. Its applications and field conditi.. |