Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.4 - 32.0 kV/mm | 290 - 813 kV/in | Average value: 16.1 kV/mm Grade Count:5 |
Overview of materials for Phenolic, Resole, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Dielectric Strength | 27.0 - 32.0 kV/mm | 686 - 813 kV/in | DIN 53481 |
Isoflon PEI Polyetherimide Materials with strong mechanical and electrical performances under high temperatures.Information provided by Isoflon. |
|||
Dielectric Strength | 16.5 - 32.0 kV/mm | 420 - 813 kV/in | Average value: 23.2 kV/mm Grade Count:17 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |