Polymer Property : Dielectric Strength = 7700 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 9.84 - 303 kV/mm
250 - 7700 kV/in
Average value: 25.4 kV/mm Grade Count:105
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..