Electrical Properties Metric English Comments
Dielectric Strength 17.7 - 135 kV/mm
450 - 3430 kV/in
Average value: 42.0 kV/mm Grade Count:40
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..