Polymer Property : Dielectric Strength = 8000 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 315 kV/mm
8000 kV/in
ASTM D1000
3M 9731 Double Coated Tape
3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other ..
Dielectric Strength 315 kV/mm
8000 kV/in
ASTM D1000
3M 9731RW Double Coated Tape
3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other ..