Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 31.1 kV/mm | 790 kV/in | ASTM D149 |
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Dielectric Strength | 31.1 kV/mm @Thickness 2.03 mm |
790 kV/in @Thickness 0.0799 in |
ASTM D149 |
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Dielectric Strength | 31.1 kV/mm | 790 kV/in | ASTM D149 |
Arlon R36798T017 0.017" (0.432 mm) Uncured Silicone Rubber with Laminated Tefzel® Substrate
(discontinue Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionAppearance: Translucent, high viscosity gum on fluoro.. |
|||
Dielectric Strength | 31.1 kV/mm | 790 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 123-40 Thermoplastic Elastomer A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Dielectric Strength | 31.1 kV/mm @Thickness 2.03 mm |
790 kV/in @Thickness 0.0799 in |
ASTM D149 |
ExxonMobil Santoprene® 251-92W232 Thermoplastic Elastomer A hard, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard.. |
|||
Dielectric Strength | 31.1 kV/mm | 790 kV/in | ASTM D149 |
Arlon 25188T017 Silicone Rubber/Laminated ETFE Film Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion |
|||
Dielectric Strength | 31.1 kV/mm | 790 kV/in | ASTM D149 |
Arlon R37208T017 0.017" (0.432 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Liner Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionThis data represents typical values for the productio.. |
|||
Dielectric Strength | 31.1 kV/mm | 790 kV/in | ASTM D149 |
Arlon 51146R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater insulationAppearance: Red sili.. |