Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.0 kV/mm | 433 kV/in | ASTM D149 |
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Dielectric Strength | 17.0 kV/mm | 433 kV/in | |
Dow Corning HV 1760/65 Silicone Rubber 65 Shore hardness high consistency silicone rubber with fast cure system and excellent tracking and erosion resistanceInformation provided by Dow Corning |
|||
Dielectric Strength | 17.0 kV/mm | 433 kV/in | |
Dow Corning HV 1760/80 SILICONE RUBBER NATURAL 80 Shore hardness high consistency silicone rubber with fast cure system and excellent tracking and erosion resistanceInformation provided by Dow Corning |