Electrical Properties Metric English Comments
Dielectric Strength 165 kV/mm
4200 kV/in
ASTM D-149
Saint-Gobain Norton® Chemfilm® DF100 Fluoropolymer Cast Film
Description: Used for Chemical Process, Electrical/Electronics, Medical, Protective/Decorative. Surface Treatments Available: Chemical Etching (1 or 2 sides). Information provided by Saint Gobain Pe..
Dielectric Strength 165 kV/mm
4200 kV/in
ASTM D-149
Saint-Gobain Norton® Chemfilm® DF110 Fluoropolymer Cast Film
Description: Used for Chemical Process, Electrical/Electronics, Medical, Protective/Decorative.Information provided by Saint Gobain Performance Products.
Dielectric Strength 165 kV/mm
4200 kV/in
ASTM D-149
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1400 Non-Conductive PTFE Tape
Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super..
Dielectric Strength 165 kV/mm
4200 kV/in
ASTM D-149
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1700 Heat Bondable PTFE Film
Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super..
Dielectric Strength 165 kV/mm
4200 kV/in
ASTM D-149
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1900 Heat Bondable PTFE Film
Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super..