Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 16.5 kV/mm | 420 kV/in | |
Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite Formerly known as grade MM 1100. Synthetic mica filler. Does not burn. Excellent radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating m.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | Cured |
Resin Technology Group UV-412 Medium Viscosity, High Clarity, UV Curable Adhesive UV 412 is a high clarity, fast setting UV adhesive. This solvent free adhesive is designed to bond a wide variety of transparent materials, (similar and dissimilar substrates). The high clarity prov.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | Cured |
Resin Technology Group UV MX-2230 Quick Fixture, Activator Cured, One-Component, Acrylic Adhesive UV MX 2230 is a one-component acrylate based polymer designed to be used as a quick-fixture, surface activated adhesive, (with optional UV or oven cure), for applications on a variety of substrates .. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6 IM 40 Z Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6 IM 435 HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUses: Low Temperature ApplicationsInformatio.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6 IM HS L BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUL File Number: E157318Processing Method: In.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6 IM L Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6 IM L W Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PET GF15 FR 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 GF33 HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Heat Stabilized, Good UV.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 GF33 L UV 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and UV Stabilizer Features: Lubricated and Good UV ResistanceInforma.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PA6/ABS 1120 GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInformation p.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | ASTM D149 |
Styron CALIBREâ„¢ 2061-22 Polycarbonate CALIBREâ„¢ 2061-22 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | ASTM D149 |
Styron CALIBREâ„¢ 301-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | ASTM D149 |
Styron EMERGEâ„¢ 4330-15 Polycarbonate EMERGEâ„¢ PC 4330-15 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | ASTM D149 |
Styron CALIBREâ„¢ 201-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | ASTM D149 |
Styron CALIBREâ„¢ 301 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | ASTM D149 |
Styron CALIBREâ„¢ 302-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | ASTM D149 |
Styron CALIBREâ„¢ 303-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | ASTM D149 |
Styron CALIBREâ„¢ 303-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | |
Tra-Con Tra-Bond 716C01 Medium Viscosity Epoxy Adhesive TRA-BOND 716C01 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications. This two-part amber adhesive is easily mixed, used and cured at room temperature.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | |
Tra-Con Tra-Bond FDA12 Food and Drug Application Epoxy Adhesive TRA-BOND FDA12 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admin.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | |
Tra-Con Tra-Bond FDA22 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-22 is a high viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admini.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | |
Tra-Con Tra-Bond FDA2YL02 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-2 YL02 is a medium viscosity epoxy resin system specifically developed for adhesive and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | ASTM D149 |
Dow CALIBRE™ MEGARAD™ 2081-15 Polycarbonate CALIBRE™ MEGARAD™ 2081-15 resin is specially formulated to meet the radiation sterilization needs of the healthcare industry, while providing exceptional clarity, heat resistance, impact strength.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | S/T |
Abatron AboCast 8103-26 High-Performance Dielectric Epoxy AboCast 8103-26 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | |
Atom Adhesives AA-BOND FDA15 Epoxy Adhesive AA-BOND FDA15 is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Administr.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | |
Atom Adhesives AA-BOND FDA2 Epoxy Adhesive AA-BOND FDA2 is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and recei.. |
|||
Dielectric Strength | 16.5 kV/mm | 420 kV/in | |
Resinlab® EP1199 Clear Unfilled Epoxy Adhesive Resinlab™ EP1199 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |