Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 16.3 kV/mm | 415 kV/in | |
Resin Technology Group TIGA 101-EX Five-Minute Epoxy Adhesive 1 part resin to 1 part hardener.TIGA 101-EX is an exceptional epoxy formulation, recommended for lower temperature or wet industrial bonding applications where fast curing is required. This clear, t.. |
|||
Dielectric Strength | 16.3 kV/mm | 415 kV/in | |
Taiwan PU Corporation TPUCO Polyurethane Sealing Resin PU sealing resin is a waterproof, insulated protective film made of quality PU resin. It is used in the prevention of humidity, germs, collision, corrosion, parts loosening, and rusting, and as ins.. |
|||
Dielectric Strength | 16.3 kV/mm | 415 kV/in | |
Tra-Con Tra-Bond 2116 Low Vapor Pressure Epoxy Staking Compound TRA-BOND 2116 is a thixotropic, low vapor pressure epoxy system that passes the NASA Outgassing Specification. It is recommended for critical electronic, aerospace, and industrial applications where.. |
|||
Dielectric Strength | 16.3 kV/mm | 415 kV/in | |
Dow Corning SLYGARD® 3-6636 SILICONE DIELECTRIC GEL KIT Two-part, transparent, LED encapsulant which is a lower-viscosity version of EG-6301.Information provided by Dow Corning |
|||
Dielectric Strength | 16.3 kV/mm | 415 kV/in | ASTM D149 |
Arlon 55272R024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use.. |