Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.2 kV/mm | 386 kV/in | 60Hz, Step-by-Step, dry; ASTM D149 |
Sumitomo Bakelite North America E 8353-706R-1 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Dielectric Strength | 15.2 kV/mm | 386 kV/in | Short Time; ASTM D149 |
Plenco 6990 Phenolic, Briquette, Compression Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Dielectric Strength | 15.2 - 16.7 kV/mm | 386 - 424 kV/in | DC Breakdown Strength |
China-Yixing Longly Refractories 99 Alumina Ceramic Tubes & Rods LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat.. |